NIZHNEKAMSKNEFTEKHIM PE 6252J (526F2) High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer NIZHNEKAMSKNEFTEKHIM Inc
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NIZHNEKAMSKNEFTEKHIM PE 6252J (526F2) High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Physical Properties Metric English Comments
Density 0.950 - 0.954 g/cc
0.0343 - 0.0345 lb/in³
Base Resin; ASTM D1505
Melt Flow 0.15 - 0.30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.15 - 0.30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1283/L
10.5 - 21 g/10 min

@Load 21.6 kg,
Temperature 190 °C
10.5 - 21 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Flow@21.6kg/Flow@2.16kg ratio > 70; ASTM D1283
Mechanical Properties Metric English Comments
Flexural Modulus >= 1.25 GPa
>= 181 ksi
ASTM D790
Izod Impact, Notched >= 2.00 J/cm
>= 3.75 ft-lb/in
ASTM D256