NIZHNEKAMSKNEFTEKHIM PE 6749F (486H6) High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer NIZHNEKAMSKNEFTEKHIM Inc
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NIZHNEKAMSKNEFTEKHIM PE 6749F (486H6) High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Physical Properties Metric English Comments
Density 0.946 - 0.950 g/cc
0.0342 - 0.0343 lb/in³
Base Resin; ASTM D1505
Melt Flow 0.50 - 0.70 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.50 - 0.70 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1283/L
9.0 - 12.6 g/10 min

@Load 21.6 kg,
Temperature 190 °C
9.0 - 12.6 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Flow@21.6kg/Flow@5kg ratio > 18; ASTM D1283