NIZHNEKAMSKNEFTEKHIM PP 8332C (EPD60R) Propylene and Ethylene Block Polymer

Category Polymer , Thermoplastic , Polyethylene (PE) , Polypropylene (PP)
Manufacturer NIZHNEKAMSKNEFTEKHIM Inc
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NIZHNEKAMSKNEFTEKHIM PP 8332C (EPD60R) Propylene and Ethylene Block Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when PP is produced, processed and PP-made articles are exploited, and improved antistatic properties to produce articles.Information provided by manufacturer
Physical Properties Metric English Comments
Melt Flow 0.30 - 0.50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.30 - 0.50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1283/L
0.50 - 0.90 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.50 - 0.90 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1283/L
1.2 - 1.9 g/10 min

@Load 5.00 kg,
Temperature 230 °C
1.2 - 1.9 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ASTM D1283/L
Mechanical Properties Metric English Comments
Flexural Modulus >= 1.05 GPa
>= 152 ksi
ASTM D790
Izod Impact, Notched >= 0.600 J/cm

@Temperature -20.0 °C
>= 1.12 ft-lb/in

@Temperature -4.00 °F
ASTM D256
>= 6.00 J/cm

@Temperature 23.0 °C
>= 11.2 ft-lb/in

@Temperature 73.4 °F
ASTM D256