Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NOVA Chemicals Novapol® PP-0118-F LLDPE Extrusion Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Extrusion Grade
Manufacturer NOVA Chemicals
Trade Name Novapol®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Novapol® PP-0118-F LLDPE Extrusion Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent ESCR, Excellent toughness, High strength, High flexibilityApplications: Pipes for pressure and non-pressure service from 12 mm to 100 mm, Potable water pipe and tubing, Underground sprinkler systems, Irrigation pipeAdditives: Antioxidants and processing stabilizersPipe properties: 1 in nominal diameter laboratory pipe SDR 13.5. Long-Term Hydrostatic Strength, Nominal: 5.5 MPa, as per ASTM D746. Compressed Ring ESCR, F50: 2500 hours minimum as per ASTM D1248.Information provided by NOVA Chemicals.
Physical Properties Metric English Comments
Density 0.918 g/cc
0.0332 lb/in³
ASTM D792
Environmental Stress Crack Resistance >= 2500 hour
>= 2500 hour
F<sub>0</sub>; Condition C, 100% Igepal; ASTM D1693
Melt Flow 1.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 58
58
ASTM D2240
Tensile Strength, Yield 10.0 MPa
1450 psi
Extension rate 2 in/min; ASTM D638
Elongation at Break 900 %
900 %
Extension rate 2 in/min; ASTM D638
Flexural Modulus 0.400 GPa
58.0 ksi
2% Strain; ASTM D3350
Izod Impact, Notched 6.80 J/cm
12.7 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 140 µm/m-°C

@Temperature 20.0 °C
77.8 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Maximum Service Temperature, Air >= 220 °C
>= 428 °F
ASTM D3350
Vicat Softening Point 104 °C
219 °F
ASTM D1525
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
ASTM D746
Users viewing this material also viewed the following: