Mechanical Properties Metric English Comments
Flexural Modulus 0.400 GPa
58.0 ksi
ASTM D790
NYCOA 7551 Copolymer Nylon Alloy
resistant to zinc chloride and other automotive fluids, good adhesion to olefins, mold & extrusion.Information provided by NYCOA, Inc.
Flexural Modulus >= 0.400 GPa
>= 58.0 ksi
ASTM D790
NIZHNEKAMSKNEFTEKHIM PE 4020R (20405) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Flexural Modulus >= 0.400 GPa
>= 58.0 ksi
ASTM D790
NIZHNEKAMSKNEFTEKHIM PE 4020W (20425) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Flexural Modulus 0.400 GPa
58.0 ksi
ASTM D790
Quadrant EPP TIVAR® Oil Filled UHMW-PE FDA/USDA Oil-Filled UHMW-PE (ASTM Product Data Sheet)
Flexural Modulus 0.400 GPa
58.0 ksi
2% Strain; ASTM D3350
NOVA Chemicals Novapol® PP-0118-F LLDPE Extrusion Resin
Excellent ESCR, Excellent toughness, High strength, High flexibilityApplications: Pipes for pressure and non-pressure service from 12 mm to 100 mm, Potable water pipe and tubing, Underground sprinkl..
Flexural Modulus 0.400 - 3.00 GPa
58.0 - 435 ksi
Average value: 2.19 GPa Grade Count:5
Overview of materials for Thermoset Polyurethane, Liquid
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Liquid". Each property range of values reported is minimum and maximum values of..
Flexural Modulus 0.400 - 16.8 GPa

@Temperature -40.0 - 200 °C
58.0 - 2440 ksi

@Temperature -40.0 - 392 °F
Average value: 5.22 GPa Grade Count:23
Overview of materials for Polyphthalamide (PPA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma..
Flexural Modulus 0.400 GPa

@Temperature 100 °C
58.0 ksi

@Temperature 212 °F
ISO 178
Solvay Specialty Polymers Amodel® AT-5001 Polyphthalamide (PPA) Resin, Dry as Molded  (discontinued **)
AMODEL AT-5001 polyphthalamide resin is a neat ductile material that offers superior retention of properties after humid thermal aging, high impact at low temperature, and better mechanical properti..
Flexural Modulus 0.400 - 1.45 GPa
58.0 - 210 ksi
Average value: 0.796 GPa Grade Count:35
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i..
Flexural Modulus 0.400 - 4.30 GPa

@Temperature -40.0 - 80.0 °C
58.0 - 624 ksi

@Temperature -40.0 - 176 °F
Average value: 2.14 GPa Grade Count:2
Overview of materials for Nylon 66, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum ..
Flexural Modulus 0.400 GPa
58.0 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP TH0300A PUR
LNP THERMOCOMP* TH0300A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity.
Flexural Modulus 0.400 GPa
58.0 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP TH0300A PUR (Asia Pacific)
LNP THERMOCOMP* TH0300A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity.
Flexural Modulus 0.400 GPa
58.0 ksi
ISO 178-1975
SIDPEC EGYPTENE® LL 2406 AA LLDPE Pipe Grade
Applications:Drip irrigation pipeSmall potable water pipeInformation provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (SIDPEC) Products
Flexural Modulus 0.400 GPa
58.0 ksi
ASTM D790
Sumitomo Chemical ESPOLEX® UT461A Thermoplastic Elastomer
ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi..
Flexural Modulus 0.400 GPa
58.0 ksi
ISO 178
Borealis Borsoft™ SD233CF High Impact Polypropylene Random Heterophasic Copolymer for Cast Film
Borsoft SD233CF is a very soft random heterophasic copolymer, suitable for use on chill roll process. The product combines unique softness with outstanding mechanical properties making it the ideal..
Flexural Modulus 0.400 GPa
58.0 ksi
DIN 53457/ISO 178
Borealis Borsoft™ SF203CF Soft Polypropylene Copolymer for Extrusion Coating
Borsoft SF203CF is a new statistic-heterophasic propylene-ethylene copolymer suitable for coating applications. Its polymer structure permits perfect adhesion to certain products. According to the..
Flexural Modulus 0.400 GPa
58.0 ksi
ASTM D790
Borealis Borstar® LE8706 Natural Bimodal LLDPE Jacketing Compound for Energy and Communication Cables
Borstar® LE8706 is a natural colorable linear low density (LLD) jacketing compound, which is produced with the Borealis proprietary Borstar® bimodal process technology. Borstar technology allows ..
Flexural Modulus 0.400 GPa
58.0 ksi
ASTM-D790
Polyram PlusTek RD120 Nylon 12, Injection Molding
Polyamide 12 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Flexural Modulus 0.400 GPa
58.0 ksi
DIN EN ISO 178
Wolf Kunststoff ZEDEX® ZX-100EL63 A1G Polymer Alloy, Elastomer Modified
Main Characteristics: Rubbery; Soft; High shock absorption; High impact resistance; Elongation > 300%Applications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automitve Technol..
Flexural Modulus 0.400 GPa
58.0 ksi
ISO 178
Borealis Borsoft™ SA233CF High Impact Polypropylene Random Heterophasic Copolymer for Blown Film
Borsoft SA233CF is a very soft random heterophasic copolymer, suitable for use on conventional blown film lines with air-coolingBorsoft SA233CF is especially suitable for soft packaging, hygienic fi..
Flexural Modulus 0.400 GPa
58.0 ksi
At 2 mm/min; ISO 178
Borealis Daplen™ AK4504 TPO Compound
Daplen AK4504 is a 30% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen AK4504 is a material with excellent impact/stiffness ratio. Thanks to its low th..
Flexural Modulus 0.400 GPa
58.0 ksi
ASTM D790
Covestro Bayflex® 110-50 Polyurethane
Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Flexural Modulus 0.400 GPa
58.0 ksi
ASTM D790
C.O.I.M. LARIPUR® LPR6560 PTMG Polyether Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..
Flexural Modulus 0.400 GPa
58.0 ksi
ASTM D790
Ashley Polymers Ashlene® L930 Nylon 12
A plasticized Nylon 12 offering improved flexibility with superior moisture and chemical resistance. The natural color is slightly darker.Data provided by the manufacturer
Flexural Modulus 0.400 GPa
58.0 ksi
ISO 178
Borealis Borstar® LE8707 Black Bimodal LLDPE Jacketing Compound for Energy and Communication Cables
Borstar® LE8707 is a black linear low density (LLD) jacketing compound, which is produced with the Borealis proprietary Borstar® bimodal process technology. Borstar® technology allows the manufa..