Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NOVA Chemicals Sclair® 31G Butene Copolymer LLDPE Extrusion Coating Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Extrusion Grade
Manufacturer NOVA Chemicals
Trade Name Sclair®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Sclair® 31G Butene Copolymer LLDPE Extrusion Coating Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
31G complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. 31G is subject to the specific limitation that it may not be used in articles used for packing or holding food during cooking.NOVA Chemicals' polyethylene resins are chemically and biologically inert.Features: Excellent tensile properties, Excellent impact toughness, Excellent processabilityAdditives: Antioxidant package
Physical Properties Metric English Comments
Density 0.922 g/cc
0.0333 lb/in³
ASTM D 792
Melt Flow 11.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
11.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Hardness, Shore D 53
53
ASTM D 2240
Tensile Strength, Yield 10.2 MPa
1480 psi
ASTM D 638
Elongation at Break 600 %
600 %
ASTM D 638
Flexural Modulus 0.335 GPa
48.6 ksi
ASTM D 790
Thermal Properties Metric English Comments
Vicat Softening Point 92.0 °C
198 °F
ASTM D 1525
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
ASTM D 746