Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.922 g/cc | 0.0333 lb/in³ | ASTM D792 |
NOVA Chemicals Novapol® LF-Y320-D Fractional Melt LDPE Film Resin Features: High melt strength and superior bubble stabilityEnhances throughputs in LLDPE blendsSuperior strength and toughnessExcellent shrink film characteristics Applications: Industrial packagingL.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | ASTM D 792 |
NOVA Chemicals Sclair® 31G Butene Copolymer LLDPE Extrusion Coating Resin 31G complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. 31G is su.. |
|||
Density | 0.922 - 0.924 g/cc | 0.0333 - 0.0334 lb/in³ | ASTM D1505 |
Petroquimica Triunfo Trithene® TS 7003 LDPE - High Strength Film The Trithene TS 7003 resin is a low-density, high molecular-weight polyethylene that offers high mechanical strength and toughness even at low temperatures. Additionally, this product is easily proc.. |
|||
Density | 0.922 - 0.924 g/cc | 0.0333 - 0.0334 lb/in³ | ASTM D1505 |
Petroquimica Triunfo Trithene® TS 7028 LDPE - Automatic Packaging The Trithene TS 7028 resin is a low-density polyethylene (LDPE) with excellent optical and processability properties that allows for the production of films combining appearance, mechanical strength.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | ExxonMobil Method |
ExxonMobil ENABLE™ EN 33330 Adhesive Resin
(discontinued **) Enable EN 33330 is a high flow, 32.5% nBA copolymer suitable for use in hot melt adhesives and sealants.Information provided by ExxonMobil Chemical |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | ASTM D1505 |
Chevron Phillips 5658 LDPE Shrink and Bundling Film Resin
(discontinued **) Resin Type: HomopolymerCharacteristics: Good Impact Strength, Good Abrasion and Tear Resistance, Good Sealing Properties, No Slip, Medium Antiblock, Easy OpenabilityApplications:Shrink Wrap, Bundlin.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | Exxon Method |
ExxonMobil Escorene® LD-102 LDPE Drawdown Resin, 1.25 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer, good clarity, laundry and dry cleaning film resin capable of providing a tough film in very thin gauges.Applications: Dry cleaning es.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® NA870252 Low Density Polyethylene ApplicationsPETROTHENE NA 870-252 exhibits an excellent balance of toughness and softness, with excellent dimensional stability. Typical applications include caps and closures, housewares, toys, co.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Catalyst CT/1-LR Polyolefin Catalyst CT/1-LR is a polyolefin based masterbatch to be used with cable silane crosslinkable compounds in the amount suggested for each material. Developed for Polidan® and Polidiemme® series.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | ASTM D1505 |
UBE F022NH Polyethylene Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | ASTM D1505 |
UBE F222NH Polyethylene Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | ASTM D1505 |
UBE F522 Polyethylene Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | ASTM D1505 |
UBE F522N Polyethylene Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | ISO 1183 |
Borealis FA7224 Low Density Polyethylene FA7224 has been developed for applications such as: Thin bags with excellent optical and slip properties, and laundry and other textile bags. Contains antioxidant.Information provided by Borealis AG.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | base resin; ISO 1183/ISO 1872-2 |
Borealis LE4201R Polyethylene Insulation Compound, Crosslinkable LE4201R is a crosslinkable natural polyethylene compound, specially designed for insulation applications. Applications LE4201R is intended for insulation of XLPE power cables with rated voltages up.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | ASTM D1505 |
Chevron Phillips MarFlex® 5628 LDPE Blown Film Resin Resin Type: HomopolymerCharacteristics: Superior tensile and impact strengthGood abrasion and tear resistanceExcellent retention of properties after agingApplications: LaminationsPallet shrinkcase s.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | ExxonMobil method |
ExxonMobil EN 33330 Ethylene n-Butyl Acrylate Copolymer Resin Product Description: ExxonMobil EN 33330 is a high flow 32.5% nBA copolymer suitable for use in hot melt adhesives and sealants. Availability: Latin America, North America and South America Additive.. |
|||
Density | 0.922 g/cc @Temperature 15.6 °C |
0.0333 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil Exterex™ A34 Synthetic Fluid Product Description: Esterex™ Adipate Esters are API category Group V fluids. These esters have excellent low-temperature properties, high viscosity indices, good lubricating properties and low vol.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | ASTM D792, ISO 1183 |
DuPont™ Fusabond® E528 Polymer Modifier DuPont™ Fusabond® E528 is a anhydride modified polyethylene. Used as a polymer modifier |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | ExxonMobil Method |
ExxonMobil LD 637.LI Molding, Extrusion and Compounding Resin Product Description: LD 637.LI is a high melt index LDPE homopolymer intended for injection molding or compounding applications requiring high flow. It is ideal for tamper-evident, tear-to-open clos.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | ASTM D792 |
Dow DOWLEX™ 2045.11G Linear Low Density Polyethylene For high speed, thin film applications Additional thermal stability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | |
Dow DOWLEX™ 2077 Linear Low Density Polyethylene, Food Grade DOWLEX® 2077 Polyethylene resin is a fully formulated linear low density polyethylene resin designed for use in food packaging applications. This blown film resin is designed to run on narrow die-g.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | |
Dow LDPE 586A Low Density Polyethylene, Packaging Grade DOW LDPE 586A resin is used for general purpose packaging applications. It contains medium levels of slip additive and low levels of antiblock additive. This material complies with U.S.FDA regulatio.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | |
Dow LDPE 640I Low Density Polyethylene, Liner Film Grade DOW LDPE 640I resin is a barefoot general purpose liner film resin for thin gauge applications requiring good drawdown and excellent toughness. This material complies with U.S.FDA regulation 21 CFR .. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | |
Dow LDPE 641I Low Density Polyethylene, Liner Film Grade DOW LDPE 641I resin is a general purpose liner film resin for thin gauge applications requiring good drawdown and excellent toughness. It contains medium levels of slip additive and low levels of an.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | |
Dow LDPE 682I Low Density Polyethylene, Film Grade DOW LDPE 682I barefoot resin is used for shrink, frozen food, and heavy duty film applications. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for food contact applications. T.. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | ASTM-D792 |
Braskem CX7020 LDPE Cast Film Extrusion Polyethylene CX7020 is a low-density polyethylene (LDPE) with excellent processability and low gel content. Those features allow for production of thin and highly uniform films. This product is identified as PE .. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | |
BASF Ethyl Acrylate Formula: C5H8O2CAS: 140-88-5Description: Acrylic acid ester suitable for the production of polymers and as a feedstock for syntheses.Applications: Ethyl acrylate forms homopolymers and copolymers. .. |
|||
Density | 0.922 g/cc | 0.0333 lb/in³ | ASTM D1505 |
Huntsman PE1059 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Excellent draw down and good processability.Applications: Film extrusion: non-abrasive packaging applications.FDA Notes: Conforms to FDA regulation 21 CFR 177.. |