Mechanical Properties Metric English Comments
Flexural Modulus 2.81 GPa
408 ksi
ASTM D790
PolyOne Geon™ Vinyl Rigid Extrusion L0152 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Flexural Modulus 2.81 GPa
408 ksi
ASTM D790
PolyOne Geon™ Vinyl Rigid Extrusion LR610 white 1046 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Flexural Modulus 2.81 GPa
408 ksi
Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790
Network Polymers MS 125 Styrene Methyl Methacrylate Terpolymer
Description: Styrene Methyl Methacrylate TerpolymerInformation provided by Network Polymers Inc.
Flexural Modulus 2.81 GPa
408 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Cycolac® MG37EPX ABS
ABS plating grade optimized for a broad processing window for both painted and plated applications. NSF standard 61 compliant (80 sq in/L)
Flexural Modulus 2.81 GPa
408 ksi
ASTM D790
Nilit Polynil® P230 High Viscosity Nylon 66
Description: Polynil P230 is a high viscosity NYLON 66 (Viscosity number 280 cm³/gr) that was developed for film- and rod extrusion. It has high melt stability and low gel content. It holds various..
Flexural Modulus 2.81 GPa
408 ksi
ASTM D790
Nilit Polynil® P240 High Viscosity Nylon 66
Description: Polynil P240 is a high viscosity NYLON 66 (Viscosity number 290 cm³/gr) that was developed for rod and slab extrusion. It has a high melt stability and a low gel content.Key characteri..
Flexural Modulus 2.81 GPa
408 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Cycoloy® CX7720 PC+ABS (Asia Pacific)
Cycoloy resin CX7720 is a non brominated and non chlorinated flame retardant PC/ABS resin grade featuring high heat resistance and thin wall FR. It is UL-94 listed at 1.2 mm V0 and 1.5mm 5VB. Its hi..
Flexural Modulus 2.81 GPa
408 ksi
ASTM D790
PolyOne Edgetek® NN-35MG/000 Black v1.1 Polyamide 66 (Nylon 66)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Flexural Modulus 2.81 GPa
408 ksi
ASTM D790
PolyOne Geon™ Vinyl Dry Blend E6755 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Flexural Modulus 2.81 GPa
408 ksi
ASTM D790
SABIC Innovative Plastics LNP FARADEX AS002 ABS
LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing 10% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding...
Flexural Modulus 2.81 GPa
408 ksi
ASTM D790
SABIC Innovative Plastics LNP FARADEX AS002 ABS (Asia Pacific)
LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Flexural Modulus 2.81 GPa
408 ksi
ASTM D790
SABIC Innovative Plastics LNP FARADEX AS002 ABS (Europe-Africa-Middle East)
LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Flexural Modulus 2.81 GPa
408 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP EL002 PEI
LNP* Lubricomp* EL002 is a compound based on Polyetherimide resin containing 10% PTFE. Added features of this material include: Internally Lubricated.
Flexural Modulus 2.81 GPa
408 ksi
2 mm/min, 64mm span; ISO 178
SABIC Innovative Plastics SABIC PPCOMPOUND 55T1030 PP
SABIC® PPcompound 55T1030 is a general purpose, talc filled, heat stabilized copolymer polypropylene compound. This compound exhibits very high impact, and is suitable for multiple processing met..
Flexural Modulus 2.81 GPa
408 ksi
ISO 178
SABIC Innovative Plastics LNP STAT-KON DX00887C PC
LNP STAT-KON* DX00887C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive.
Flexural Modulus 2.81 GPa
408 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP DX09402 PC
LNP* THERMOCOMP* DX09402 is a compound based on Polycarbonate containing Proprietary Filler(s).
Flexural Modulus 2.81 GPa
408 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOTUF MX00619 PP
LNP* Thermotuf* MX00619 is a compound based on Polypropylene resin containing Proprietary Filler(s).
Flexural Modulus 2.81 GPa
408 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOTUF MX00619 PP (Asia Pacific)
LNP* Thermotuf* MX00619 is a compound based on Polypropylene resin containing Proprietary Filler(s).
Copyright © lookpolymers.com All Rights Reserved