North Wood Plastics PS with 60% Wood Fiber

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Wood Filled
Manufacturer North Wood Plastics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF North Wood Plastics PS with 60% Wood Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by North Wood Plastics, Inc.
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
Estimated by MatWeb
Linear Mold Shrinkage 0.00010 cm/cm
0.00010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 28.0 MPa
4060 psi
ASTM D638
Tensile Strength, Yield 28.0 MPa
4060 psi
ASTM D638
Flexural Modulus 8.30 GPa
1200 ksi
ASTM D790
Thermal Properties Metric English Comments
CTE, linear 22.0 µm/m-°C

@Temperature 20.0 °C
12.2 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 1.8 MPa (264 psi) 68.0 °C
154 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature <= 200 °C
<= 392 °F
To prevent fiber degradation.