Nylene® 600 Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Extruded
Manufacturer Nylene®
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nylene® 600 Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Dry as molded. Extrusion grade. Nylene 600 is a general purpose, medium viscosity, extrusion grade resin used in applications such as rods, slabs, and tubing. Other applications include wire jacketing and centrifugal casting which require good dielectric properties, toughness, and fatigue resistance. Optimum processing conditions should provide a melt temperature of 480 - 500ºF at the die.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Water Absorption 1.9 %
1.9 %
Mechanical Properties Metric English Comments
Tensile Strength, Yield 83.0 MPa
12000 psi
ASTM D638
Elongation at Break 70 %
70 %
ASTM D638
Flexural Yield Strength 102 MPa
14800 psi
ASTM D790
Izod Impact, Notched 0.400 J/cm
0.749 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 175 °C
347 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
167 °F
ASTM D648
Flammability, UL94 V-2
V-2
Processing Properties Metric English Comments
Processing Temperature 255 °C
491 °F