Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Nylene® 609 Nylon 6, 50% RH, Film/Extrusion Grade

Category Polymer , Film , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Film Grade
Manufacturer Nylene®
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nylene® 609 Nylon 6, 50% RH, Film/Extrusion Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Film Grade. Nylene 609 is a high viscosity, extrusion resin recommended for practically all types of extrusion including profile, film, and extrusion coating. It is especially recommended for flexible packaging where as a film or coating it is used for the outside layer in multi-ply film constructions. Nylene 609 has excellent melt flow and melt strength properties. Optimum processing conditions should permit for a melt temperature of 550 - 575ºF at the die.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 61.0 MPa
8850 psi
ASTM D638
Elongation at Break 285 %
285 %
ASTM D638
Flexural Yield Strength 39.0 MPa
5660 psi
ASTM D790
Izod Impact, Notched 3.10 J/cm
5.81 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 151 °C
304 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
167 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 295 °C
563 °F
Users viewing this material also viewed the following: