Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 235 °C | 455 °F | ASTM D3418 |
Nylene® 6111 (HS) , 40% Glass/Mineral Reinforced Nylon 6/6 Description: Nylene® 6111 (HS) is a 40% mineral reinforced, impact modified nylon 6/6. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Pol.. |
|||
Melting Point | 235 °C | 455 °F | ASTM D3418 |
Nylene® 9633 , 33% Glass Reinforced Nylon 6,6/6 Description: Nylene® 9633 is a 33% glass fiber reinforced specialty nylon. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resou.. |
|||
Melting Point | 235 °C | 455 °F | ASTM D3418 |
Nylene® 9643 , 43% Glass Reinforced Nylon 6,6/6 Description: Nylene® 9643 is a 43 % glass fiber reinforced specialty nylon. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Reso.. |
|||
Melting Point | 235 - 310 °C | 455 - 590 °F | Average value: 258 °C Grade Count:38 |
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl.. |
|||
Melting Point | 235 - 263 °C | 455 - 505 °F | Average value: 254 °C Grade Count:9 |
Overview of materials for Nylon 66/Nylon 6 Blend, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/Nylon 6 Blend, Glass Fiber Filled". Each property range of values reported is minimum and maxim.. |
|||
Melting Point | 235 - 240 °C | 455 - 464 °F | |
Indium Corp. Indalloy® 133 Sn-Sb Solder Alloy Higher tensile strength solder than #121. Particular application is joining copper tubing in refrigeration and potable water systems. Has good wettability with good long time sheer strength at 100Â.. |
|||
Melting Point | 235 - 245 °C | 455 - 473 °F | Sheath Melt Point; LCL-PR29 |
Intercontinental Polymers 1613 Bicomponent PBN/PET Fiber Type - 1.8 Denier X 3.0 Inches 50/50 PBN Sheath/PET Core. Luster: Semi-Dull. Finish: Hydrophilic.Applications of bicomponent polyester fiber: Absorbent products, hygiene products, non-wovens, filtration, sliver knit, microdenie.. |
|||
Melting Point | 235 °C | 455 °F | DSC |
Westlake Plastics PMP Film Made from TPX® Polymethylpentene Resin Lowest specific gravity of any known thermoplastic. Exceptional electrical properties. Good chemical resistance. High heat resistance. Excellent acoustical properties. Transparency. FDA compli.. |
|||
Melting Point | 235 °C | 455 °F | |
Williams Advanced Alloys WS235 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Melting Point | 235 °C | 455 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® G4V-5H black 9915 PA*-GF50 Product description: Grivory G4V-5H is a 50% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline partially aromatic copolyamide. Grivory G4V-5H is used for injectio.. |
|||
Melting Point | 235 °C | 455 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® G4V-5H nat PA*-GF50 Product description: Grivory G4V-5H is a 50% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline partially aromatic copolyamide. Grivory G4V-5H is used for injectio.. |
|||
Melting Point | <= 235 °C | <= 455 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 071.LQ Low Density Polyethylene Resin Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tough.. |
|||
Melting Point | <= 235 °C | <= 455 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 071.LR Low Density Polyethylene Resin Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tough.. |
|||
Melting Point | <= 235 °C | <= 455 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 156BW Low Density Polyethylene Resin Product Description: LD 156 series are LDPE grades, specially designed for lamination films and co-extruded films. They offer good mechanical, stiffness and optical properties, combined with very lo.. |
|||
Melting Point | <= 235 °C | <= 455 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 156HE Low Density Polyethylene Resin Product Description: LD 156 series are LDPE grades, specially designed for lamination films and co-extruded films. They offer good mechanical, stiffness and optical properties, combined with very lo.. |
|||
Melting Point | 235 °C | 455 °F | ISO 11357-3 |
Ascend Performance Materials Vydyne® 86XFS Nylon 66/6 Vydyne® 86XFS is a medium-viscosity PA66/6 random copolymer used for extrusion-compounding. This copolymer is specifically designed to be used with FR packages and high mineral loadings due to its .. |
|||
Melting Point | 235 °C | 455 °F | ASTM D789 |
Aclo Accucomp Nylon 6 NY0700L |
|||
Melting Point | 235 °C | 455 °F | ISO 11357-1/-2 |
BASF Ultradur® B 4040 G10 50% Glass Filled BK 15029 PBT + PET Description: Injection molding grade with 50% glass fibers for industrial parts with excellent surface quality, for example external door handles in vehicles, visible sunroof frames, oven door handl.. |
|||
Melting Point | 235 °C | 455 °F | 10K/min; ISO 3146 |
CENTROPLAST CENTROSOL Acrylonitrile butadiene Styrene copolymer CENTROSOL ABS has high rigidity and hardness even at low temperatures. It is scratch resistant, non-toxic, with high surface resistance. It is used in operation components for electrical equipment .. |
|||
Melting Point | 235 °C | 455 °F | MPC Method |
Mitsui TPX® MX002 Methylpentene Copolymer TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi.. |