Nylene® NX4301 Nylon 6, Extrusion Grade

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Extruded
Manufacturer Nylene®
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nylene® NX4301 Nylon 6, Extrusion Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Dry as molded. Extrusion grade. Nylene NX4301 is a high viscosity, UV stabilized extrusion grade nylon resistant to degradation by ultraviolet light. The elevated quality of UV resistance is attributed to highly uniform dispersion of 2% carbon black. With an ASTM viscosity of 200, NX4301 has very good melt flow and melt strength characteristics which are important for profile extrusion. Optimum processing conditions should permit for a melt temperature of 550 - 575ºF at the die.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 70.0 MPa
10200 psi
ASTM D638
Elongation at Break 140 %
140 %
ASTM D638
Flexural Yield Strength 120 MPa
17400 psi
ASTM D790
Izod Impact, Notched 0.500 J/cm
0.937 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °C
144 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 295 °C
563 °F