Material Notes:
Description: Naxel™ PC43 is a medium flow, UV resistant polycarbonate. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
Melt Flow 12 g/10 min
12 g/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 62.1 MPa
9000 psi
ASTM D638
Elongation at Break 100 %
100 %
ASTM D638
Flexural Modulus 2.24 GPa
325 ksi
ASTM D790
Izod Impact, Notched 8.01 J/cm
15.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 129 °C
265 °F
ASTM D648
Users viewing this material also viewed the following: