Nylene® PA6/6 Homopolymer 134 HSL Nylon 6/6

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Nucleated
Manufacturer Nylene®
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nylene® PA6/6 Homopolymer 134 HSL Nylon 6/6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low Viscosity Nucleated Grade; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 90.0 MPa
13100 psi
ASTM D638
Elongation at Break 30 %
30 %
ASTM D638
Flexural Modulus 3.25 GPa
471 ksi
ASTM D790
Izod Impact, Notched 0.400 J/cm
0.749 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 254 °C
489 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 235 °C
455 °F
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
ASTM D648