Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ovation Polymers Nemcon™ H PC DP113/X5 Polycarbonate

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer Ovation Polymers
Trade Name Nemcon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ovation Polymers Nemcon™ H PC DP113/X5 Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polycarbonate-Thermally conducting, electrically insulating grade with high HDT and improved processability.Information provided by Ovation Polymers
Physical Properties Metric English Comments
Specific Gravity 1.56 g/cc
1.56 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 45.0 MPa
6530 psi
50 mm/min; ASTM D638
Elongation at Break 3.45 %
3.45 %
50 mm/min; ASTM D638
Tensile Modulus 2.45 GPa
355 ksi
50 mm/min; ASTM D638
Flexural Strength 75.0 MPa
10900 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.95 GPa
428 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.587 J/cm

@Temperature 23.0 °C
1.10 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Thermal Conductivity 1.80 W/m-K
12.5 BTU-in/hr-ft²-°F
ASTM E-1461
Deflection Temperature at 1.8 MPa (264 psi) 124 °C

@Thickness 3.20 mm
255 °F

@Thickness 0.126 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Surface Resistivity per Square 1.00e+12 ohm
1.00e+12 ohm
ASTM D257
Users viewing this material also viewed the following: