Material Notes:
Thermally Conductive Polyetheretherketone, excellent chemical, high stiffness, modulus and HDT.Information provided by Ovation Polymers
Physical Properties Metric English Comments
Specific Gravity 1.52 g/cc
1.52 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 75.0 MPa
10900 psi
50 mm/min; ASTM D638
Elongation at Break 2.5 %
2.5 %
50 mm/min; ASTM D638
Tensile Modulus 6.25 GPa
906 ksi
50 mm/min; ASTM D638
Flexural Yield Strength 135 MPa
19600 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 7.05 GPa
1020 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.325 J/cm

@Temperature 23.0 °C
0.609 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Thermal Conductivity 3.10 W/m-K
21.5 BTU-in/hr-ft²-°F
ASTM E-1461
Deflection Temperature at 1.8 MPa (264 psi) 206 °C

@Thickness 3.20 mm
403 °F

@Thickness 0.126 in
unannealed; ASTM D648
Glass Transition Temp, Tg 150 °C
302 °F
ASTM D3482
Electrical Properties Metric English Comments
Surface Resistivity per Square 8.00e+12 ohm
8.00e+12 ohm
ASTM D257