Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Nylon 612 with PTFE Filler

Category Polymer , Thermoplastic , Nylon , Nylon 612 , Nylon 612 with PTFE Filler
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Nylon 612 with PTFE Filler.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612 with PTFE Filler". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.12 - 1.37 g/cc
0.0405 - 0.0495 lb/in³
Average value: 1.19 g/cc Grade Count:15
Water Absorption 0.140 - 0.500 %
0.140 - 0.500 %
Average value: 0.274 % Grade Count:7
Linear Mold Shrinkage 0.00200 - 0.0400 cm/cm
0.00200 - 0.0400 in/in
Average value: 0.0180 cm/cm Grade Count:15
Mechanical Properties Metric English Comments
Hardness, Rockwell R 109 - 121
109 - 121
Average value: 116 Grade Count:5
Tensile Strength, Ultimate 44.8 - 131 MPa
6500 - 19000 psi
Average value: 55.4 MPa Grade Count:15
Elongation at Break 2.00 - 30.0 %
2.00 - 30.0 %
Average value: 9.07 % Grade Count:15
Modulus of Elasticity 1.86 - 8.96 GPa
270 - 1300 ksi
Average value: 2.71 GPa Grade Count:14
Flexural Yield Strength 62.1 - 200 MPa
9000 - 29000 psi
Average value: 79.9 MPa Grade Count:14
Flexural Modulus 1.72 - 7.58 GPa
250 - 1100 ksi
Average value: 2.46 GPa Grade Count:14
Izod Impact, Notched 0.427 - 1.07 J/cm
0.800 - 2.00 ft-lb/in
Average value: 0.532 J/cm Grade Count:15
Izod Impact, Unnotched 3.20 - 12.8 J/cm
6.00 - 24.0 ft-lb/in
Average value: 6.45 J/cm Grade Count:13
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 121 - 218 °C
250 - 425 °F
Average value: 183 °C Grade Count:6
Deflection Temperature at 1.8 MPa (264 psi) 74.0 - 216 °C
165 - 420 °F
Average value: 96.5 °C Grade Count:13
Flammability, UL94 HB
HB
Grade Count:11
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+13 - 1.00e+15 ohm-cm
1.00e+13 - 1.00e+15 ohm-cm
Average value: 2.26e+14 ohm-cm Grade Count:5
Processing Properties Metric English Comments
Processing Temperature 252 - 279 °C
485 - 535 °F
Average value: 266 °C Grade Count:6
Melt Temperature 232 - 285 °C
450 - 545 °F
Average value: 263 °C Grade Count:8
Mold Temperature 49.0 - 107 °C
120 - 225 °F
Average value: 77.5 °C Grade Count:14
Drying Temperature 79.4 - 107 °C
175 - 225 °F
Average value: 82.3 °C Grade Count:8
Moisture Content 0.200 %
0.200 %
Average value: 0.200 % Grade Count:6
Dew Point -17.8 °C
0.000 °F
Average value: -17.8 °C Grade Count:6
Injection Pressure 68.9 - 124 MPa
10000 - 18000 psi
Average value: 96.5 MPa Grade Count:12