Linear Mold Shrinkage 0.00120 - 0.0400 cm/cm
0.00120 - 0.0400 in/in
Average value: 0.0207 cm/cm Grade Count:256
Overview of materials for Acetal Copolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of..
Linear Mold Shrinkage 0.00330 - 0.0400 cm/cm
0.00330 - 0.0400 in/in
Average value: 0.0203 cm/cm Grade Count:116
Overview of materials for Acetal Homopolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values ..
Linear Mold Shrinkage 0.00200 - 0.0400 cm/cm
0.00200 - 0.0400 in/in
Average value: 0.0108 cm/cm Grade Count:35
Overview of materials for Polypropylene, Mineral Reinforced, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced, Impact Modified". Each property range of values reported is minimum a..
Linear Mold Shrinkage 0.0300 - 0.0400 cm/cm
0.0300 - 0.0400 in/in
Average value: 0.0350 cm/cm Grade Count:10
Overview of materials for Modified ETFE, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Modified ETFE, Unreinforced". Each property range of values reported is minimum and maximum values of ap..
Linear Mold Shrinkage 0.00200 - 0.0400 cm/cm
0.00200 - 0.0400 in/in
Average value: 0.0180 cm/cm Grade Count:15
Overview of materials for Nylon 612 with PTFE Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612 with PTFE Filler". Each property range of values reported is minimum and maximum values of app..
Linear Mold Shrinkage 0.00800 - 0.0400 cm/cm
0.00800 - 0.0400 in/in
Average value: 0.0192 cm/cm Grade Count:26
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Injection Molded". Each property range of values reported is minimum a..
Linear Mold Shrinkage 0.00200 - 0.0400 cm/cm
0.00200 - 0.0400 in/in
Average value: 0.0160 cm/cm Grade Count:109
Overview of materials for Nylon 66, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri..
Linear Mold Shrinkage 0.00300 - 0.0400 cm/cm
0.00300 - 0.0400 in/in
Average value: 0.0174 cm/cm Grade Count:39
Overview of materials for Acetal Copolymer, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu..
Linear Mold Shrinkage 0.00480 - 0.0400 cm/cm
0.00480 - 0.0400 in/in
Average value: 0.0197 cm/cm Grade Count:97
Overview of materials for Acetal Copolymer, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of ..
Linear Mold Shrinkage 0.0100 - 0.0400 cm/cm
0.0100 - 0.0400 in/in
Average value: 0.0346 cm/cm Grade Count:102
Overview of materials for Polypropylene, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appr..
Linear Mold Shrinkage 0.00200 - 0.0400 cm/cm
0.00200 - 0.0400 in/in
Average value: 0.0125 cm/cm Grade Count:44
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum ..
Linear Mold Shrinkage 0.000 - 0.0400 cm/cm
0.000 - 0.0400 in/in
Average value: 0.00583 cm/cm Grade Count:27
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported..