Material Notes:
Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics cooling applications. These versatile liquid reactive materials can be dispensed and cured into complex geometries for cooling of multi-height components on a PCB without the expense of a molded sheet. Each compound is available in ready-to-use cartridge systems, eliminating weighing, mixing, and degassing procedures.Product Attributes: One-component moisture-cure RTV, supplied with primer 1086 (primer is not required for cure but promotes adhesion) and Non-acetic acid generatingInformation provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 2.10 g/cc
2.10 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 56
56
ASTM D2240
Thermal Properties Metric English Comments
CTE, linear 150 µm/m-°C
83.3 µin/in-°F
ASTM E831
Specific Heat Capacity 1.00 J/g-°C
0.239 BTU/lb-°F
ASTM E1269
Thermal Conductivity 0.900 W/m-K
6.25 BTU-in/hr-ft²-°F
ASTM D5470
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -70.0 °C
-94.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
ASTM D257
Dielectric Constant 3.9

@Frequency 1.00e+6 Hz
3.9

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 20.0 kV/mm
508 kV/in
ASTM D149
Dissipation Factor 0.010

@Frequency 1.00e+6 Hz
0.010

@Frequency 1.00e+6 Hz
Chomerics
Processing Properties Metric English Comments
Cure Time 2880 min

@Temperature 23.0 °C
48.0 hour

@Temperature 73.4 °F
50% RH
Pot Life 30.0 min

@Temperature 23.0 °C
30.0 min

@Temperature 73.4 °F
2X Starting Viscosity
Shelf Life 6.00 Month
6.00 Month
From date of Manufacture
Descriptive Properties Value Comments
Binder Silicone
Color White
Filler Aluminum Oxide
Mix Ratio 100:3
Number of Components 1-part