Material Notes:
Description: This is a silver filled epoxy system designed for maximum performance and lowest volume resistivity. It is easily mixed 1:1 by volume or weight, from the two one-ounce jars. Its consistency is that of a thick paste, making it easy to dispense and apply.Information provided by Chomerics
Mechanical Properties Metric English Comments
Shear Strength >= 9.65 MPa
>= 1400 psi
Cured; ASTM D1002
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 149 °C
300 °F
Cured
Minimum Service Temperature, Air -62.0 °C
-79.6 °F
Cured
Shrinkage <= 1.0 %
<= 1.0 %
Cured
Electrical Properties Metric English Comments
Volume Resistivity <= 0.0010 ohm-cm
<= 0.0010 ohm-cm
Cured; QAP-1017
Processing Properties Metric English Comments
Cure Time 30.0 min

@Temperature 100 °C
0.500 hour

@Temperature 212 °F
Recommended Cure
30.0 min

@Temperature 100 °C
0.500 hour

@Temperature 212 °F
Followed by 24 hrs @ RT
Pot Life 45 min

@Temperature 25.0 °C
45 min

@Temperature 77.0 °F
Shelf Life 15.0 Month
15.0 Month
Unopened Container
Descriptive Properties Value Comments
Color Bright Silver
Consistency Thick Paste
Filler Ag
Final Condition Rigid
Mix Ratio 1:1
Number of Components Two
Resin Epoxy
Volume 1.5 in3
Weight 2 oz
Users viewing this material also viewed the following: