Material Notes:
COPYLENE™ CH020S is a polypropylene homopolymer resin typically used by customers for BOPP (biaxially oriented polypropylene) Applications: Film ExtrusionInformation provided by Phillips 66.
Physical Properties Metric English Comments
Density 0.902 g/cc
0.0326 lb/in³
ASTM D792
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 33.1 MPa
4800 psi
(2 in/min); ASTM D638
Elongation at Yield 11.9 %
11.9 %
ASTM D638
Flexural Modulus 1.35 GPa
196 ksi
0.05 in/mm, 1% Secant, Procedure A; ASTM D790
Descriptive Properties Value Comments
Process Film