Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 33.1 MPa | 4800 psi | 2 in per min; ASTM D638 |
Network Polymers NPP 25-0216 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | 2 in/min; ASTM D638 |
Phillips 66 COPYLENE® CH200L Polypropylene, Homopolymer, CR, Antistat, Injection Molding COPYLENE™ CH200L is designed for general purpose injection molding applications with anti-static and controlled rheology. Applications: Food Containers, Housewares, Closures.Information provided by.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | 2 in/min; ASTM D638 |
Phillips 66 COPYLENE® CH020-02 Polypropylene, Thermoforming, Sheet, Film COPYLENE™ CH020-02 is a polypropylene homopolymer resin suitable for thermoforming, sheet and film fiber applications. Applications: Opaque Containers. Equivalent to Pro-fax® HL783HInformation pro.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | (2 in/min); ASTM D638 |
Phillips 66 COPYLENE® CH020S Polypropylene, Homopolymer, BOPP COPYLENE™ CH020S is a polypropylene homopolymer resin typically used by customers for BOPP (biaxially oriented polypropylene) Applications: Film ExtrusionInformation provided by Phillips 66. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | 2 in/min; ASTM D638 |
Phillips 66 COPYLENE® CH034 Polypropylene, Homopolymer, BOPP COPYLENE™ CH034, a polypropylene homopolymer resin, is designed for the production of biaxially oriented polypropylene films (BOPP). Potential uses include metalized film applications, (either dire.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
M. Holland Company PP100 Polypropylene Homopolymer, General Purpose High clarityHomopolymerGood melt strengthHigh tensile strengthApplications: Thin-walled partsSheetStrapping |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
Global TPP-120 20% Talc Filled Polypropylene Information provided by Global Polymers Corporation. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
LTL Color Compounds ColorRxâ„¢ PP1-2000RX Biocompatible Polypropylene Homopolymer A biocompatible 20 melt injection molding grade of Polypropylene homopolymer for healthcare applications.All information provided by LTL Color Compounders, Inc. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
LTL Color Compounds ColorRxâ„¢ PP1-2002ARX Biocompatible Polypropylene Homopolymer A biocompatible 20 melt injection molding grade of Polypropylene homopolymer for healthcare applications, containing antimicrobial protection.All information provided by LTL Color Compounders, Inc. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
Fiberfil® J-68/10/E Polypropylene Copolymer, 10% Glass Fiber Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
Techmer ES HiFill® HDPE MM40 40% Mica Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mica Filler, 40% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
Spartech Royalite R21 ABS General Purpose Sheet Description: General Purpose SheetInformation provided by Spartech. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
Techmer ES HiFill® PP 0096 S2 LE Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: Low ExtractablesInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
Techmer ES HiFill® PP 0096 S3 Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
Techmer ES Plastiblend® ABS 8007 Availability: North AmericaForms: PelletsFeatures: General Purpose and High FlowInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
A. Schulman PP 1247-01 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 1247-01 is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness. ApplicationPolypropylene PP 12.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
A. Schulman PP 1449-01 Polypropylene General-Purpose Homopolymer Polypropylene DescriptionPolypropylene PP 1449-01 Natural is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness.ApplicationPP 1449-01 m.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
A. Schulman PP 1247-01 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 1247-01 is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness. ApplicationPolypropylene PP 12.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
A. Schulman PP 1449-01 Polypropylene General-Purpose Homopolymer Polypropylene DescriptionPolypropylene PP 1449-01 Natural is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness.ApplicationPP 1449-01 m.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
A. Schulman PP 1449-01 Polypropylene General-Purpose Homopolymer Polypropylene DescriptionPolypropylene PP 1449-01 Natural is a homopolymer polypropylene designed for general-purpose injection-molding applications where parts require excellent stiffness.ApplicationPP 1449-01 m.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
Eastman Tenite Butyrate 285A2R30010 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
Eastman Tenite Butyrate 285A3720010 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
Eastman Tenite Butyrate 485E2R30010 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
Eastman Tenite Butyrate 565A2R30016 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
Eastman Tenite Butyrate 576E3720010 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D412 |
ACC EP RAP-1567 SP-HX EPI Engineered Polymers Silicone Aliphatic Polyurea RAP-1567 SP is a two component 100% solids, no VOC’s, silicone aliphatic polyureas “Powered by ReactAmine® Technology” that was developed for UV stable (colorfast) polyurea applications. This ne.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D-638 |
Bapolene® 4072 Polypropylene, Injection Grade Bapolene PP4072 is a high flow, fast cycle injection molding resin. This product meets FDA standards for food contact applications.Applications: Appliances, containers, and thin-walled articles.Bap.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | 50 mm/min; ASTM D638 |
Amco PRIMATOP PP HOMO 011 Extrusion Processing Polypropylene PP HOMO 011 features high molecular weight, high isotactic, and does not contain slip or anti-block. Applications include strapping, various extrusion profile, and sheet and film applications.Former.. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | ASTM D638 |
Birch Plastics RPP1215 Recycled Polypropylene RPP1215 is a homopolymer polypropylene reprocessed pellets made from 100% post industrial recycled material made for injection molding applications.Information provided by Birch Plastics, Inc. |
|||
Tensile Strength, Yield | 33.1 MPa | 4800 psi | 2" (50mm) per min.; ASTM D638 |
Formosa Plastics Formolene® 4100N Injection Molding Polypropylene Homopolymer with ESCR AdditivesApplications: Closures, small appliances, housewares and toys.Formolene 4100N is a medium viscosity, highly isotactic polypropylene homopolymer designed for various in.. |