Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plaskolite West Optix® CA-1000 I Clear High Impact Acrylic Resin

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic, Impact Modified, Molded
Manufacturer Plaskolite West, Inc.
Trade Name Optix®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plaskolite West Optix® CA-1000 I Clear High Impact Acrylic Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High impact acrylic resin, injection molding gradeApplications: A high-impact acrylic resin for injection molding. This resin offers impact strengths up to ten times of general-purpose acrylic resins. Can be used for FDA food use or USP medical use. (Meets FDA CFR-21 Sec 177.1010 for food use. Meets USP Plastic Class VI for medical use.).
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
ASTM D792
Melt Flow 2.8 g/10 min
2.8 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 42.1 MPa
6110 psi
ASTM D638
Elongation at Break 14 %
14 %
ASTM D638
Modulus of Elasticity 2.03 GPa
294 ksi
ASTM D638
Flexural Strength 61.4 MPa
8910 psi
ASTM D790
Izod Impact, Notched 0.590 J/cm
1.11 ft-lb/in
ASTM D256
Impact Test 5.50 J
4.06 ft-lb
Falling weight impact per ASTM D3029 GB
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °C
172 °F
ASTM D648
Vicat Softening Point 108 °C
226 °F
Rate A, ASTM D1525
Flammability, UL94 HB
HB
Optical Properties Metric English Comments
Transmission, Visible 90.8 %
90.8 %
ASTM D1003