Plaskolite West Optix® CA-61 Clear UV General Purpose Acrylic Resin

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic, General Purpose, Molded
Manufacturer Plaskolite West, Inc.
Trade Name Optix®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plaskolite West Optix® CA-61 Clear UV General Purpose Acrylic Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General purpose acrylic resin, injection molding and extrusion gradeApplications: A general-purpose acrylic resin designed primarily for injection molding. This resin offers a medium melt flow rate with good heat resistance.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
Melt Flow 6.0 g/10 min
6.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 66.2 MPa
9600 psi
ASTM D638
Elongation at Break 3.4 %
3.4 %
ASTM D638
Modulus of Elasticity 3.03 GPa
439 ksi
ASTM D638
Flexural Strength 107.6 MPa
15610 psi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 91.0 °C
196 °F
ASTM D648
Vicat Softening Point 102 °C
216 °F
Rate A, ASTM D1525
Flammability, UL94 HB
HB
Optical Properties Metric English Comments
Transmission, Visible 92 %
92 %
ASTM D1003