Material Notes:
Injection Molding Grade Pellets. Better impact strength than CA-924. Excellent surface gloss, optical clarity, and practical toughness.
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
ASTM D792
Melt Flow 4.5 g/10 min
4.5 g/10 min
Condition 230/3.8; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 50.0 MPa
7250 psi
ASTM D638
Elongation at Break 5.3 %
5.3 %
ASTM D638
Modulus of Elasticity 2.00 GPa
290 ksi
ASTM D638
Flexural Strength 76.0 MPa
11000 psi
ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Gardner Impact 3.30 J
2.43 ft-lb
ASTM D3029 GB
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C
174 °F
ASTM D648
Vicat Softening Point 112 °C
234 °F
ASTM D1525
Flammability, UL94 HB
HB
Optical Properties Metric English Comments
Transmission, Visible 91.3 %
91.3 %
Luminous Transmittance, ASTM D1003
Processing Properties Metric English Comments
Melt Temperature 221 - 254 °C
430 - 489 °F