Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plastcom SLOVALEN PH 66 GF 30 FRO 4 PP, 30% glass fibre, mod. of mech. prop.

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Glass Reinforced, Impact Modified
Manufacturer Plastcom spol. s r.o.
Trade Name SLOVALEN
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastcom SLOVALEN PH 66 GF 30 FRO 4 PP, 30% glass fibre, mod. of mech. prop..pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
Linear Mold Shrinkage 0.0068 cm/cm
0.0068 in/in
Linear Mold Shrinkage, Transverse 0.0111 cm/cm
0.0111 in/in
Melt Flow 3.0 g/10 min

@Load 0.325 kg,
Temperature 270 °C
3.0 g/10 min

@Load 0.716 lb,
Temperature 518 °F
Mechanical Properties Metric English Comments
Tensile Strength at Break 65.0 MPa
9430 psi
Elongation at Break 2.0 %
2.0 %
Tensile Modulus 5.90 GPa
856 ksi
Flexural Strength 110 MPa
16000 psi
Flexural Modulus 5.60 GPa
812 ksi
Charpy Impact Unnotched 3.70 J/cm²

@Temperature -20.0 °C
17.6 ft-lb/in²

@Temperature -4.00 °F
3.90 J/cm²

@Temperature 23.0 °C
18.6 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 0.600 J/cm²

@Temperature -20.0 °C
2.86 ft-lb/in²

@Temperature -4.00 °F
0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 160 °C
320 °F
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
Vicat Softening Point 163 °C
325 °F
B
Flammability, UL94 V-0
V-0
Glow Wire Test 960 °C
1760 °F
Processing Properties Metric English Comments
Melt Temperature 200 - 250 °C
392 - 482 °F
Mold Temperature 40.0 - 80.0 °C
104 - 176 °F
Injection Pressure 70.0 - 120 MPa
10200 - 17400 psi
Users viewing this material also viewed the following: