Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plastcom SLOVAMID 66 GB 20 LS PA66, 20% glass beads, light stability

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass Bead Filled
Manufacturer Plastcom spol. s r.o.
Trade Name SLOVAMID 66
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastcom SLOVAMID 66 GB 20 LS PA66, 20% glass beads, light stability.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FeaturesPA 66 for injection moulding, chemically reinforced with 20 % glass beads, light stabilized, suitable for high strength and high impacted mouldings. Used in automotive, engineering and electrical industry. Can be used in environment, in which longtime heat impact of up to 200°C occurs. Decrease in tensile strength by 50 % after 5000 hours at 170°C. The heat stabilization predetermines the products to environment with longtime heat exposure.Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
Viscosity Measurement 1.55 - 1.66
1.55 - 1.66
Linear Mold Shrinkage 0.0155 cm/cm
0.0155 in/in
Linear Mold Shrinkage, Transverse 0.0166 cm/cm
0.0166 in/in
Melt Flow 3.0 g/10 min

@Load 0.325 kg,
Temperature 270 °C
3.0 g/10 min

@Load 0.716 lb,
Temperature 518 °F
Mechanical Properties Metric English Comments
Tensile Strength at Break 45.0 MPa
6530 psi
Elongation at Break 20 %
20 %
Tensile Modulus 3.10 GPa
450 ksi
Flexural Strength 65.0 MPa
9430 psi
Flexural Modulus 2.50 GPa
363 ksi
Charpy Impact Unnotched 4.00 J/cm²

@Temperature 23.0 °C
19.0 ft-lb/in²

@Temperature 73.4 °F
4.00 J/cm²

@Temperature -20.0 °C
19.0 ft-lb/in²

@Temperature -4.00 °F
Charpy Impact, Notched 0.100 J/cm²

@Temperature -20.0 °C
0.476 ft-lb/in²

@Temperature -4.00 °F
0.200 J/cm²

@Temperature 23.0 °C
0.952 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
482 °F
Vicat Softening Point 250 °C
482 °F
B
Flammability, UL94 HB
HB
Glow Wire Test 650 °C
1200 °F
Processing Properties Metric English Comments
Melt Temperature 280 - 300 °C
536 - 572 °F
Mold Temperature 60.0 - 90.0 °C
140 - 194 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 4 hour
4 hour
Moisture Content 0.15 %
0.15 %
Injection Pressure 70.0 - 120 MPa
10200 - 17400 psi