Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.100 J/cm² @Temperature 23.0 °C |
0.476 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom PLASTAMID® 66 BT N 32 C PA66 PA66 basic type for injection molding, compounding, extrusion. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fasteners, clamps, hobby tools, toys. Delivere.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PC 51 C 40 LS/1M Polypropylene reinforced with mineral filler, UV stabilized Modified copolymer PP for injection molding with the content of 40% mineral filler, UV stabilized. Product meets glow wire test at 750°C. Delivered in full RAL color scale.Information Provided by P.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PC 51 GF 10 PP, 10% glass fibre FeaturesModified copolymer PP for injection moulding, chemically reinforced with 10% glass fibre, with high strength, rigidity and toughness, adapted thermal properties, decreased shrinkage. Suitabl.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PC 78 FRT 5 PP, glass fibre, mod. of mech. properties FeaturesModified copolymer PP for injection moulding, contains the modifier of mechanical properties and non halogen and free phosphor flame retardant. Increased strength in comparison with unfilled.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PH 51 C 40 Polypropylene Homopolymer and Copolymer, 40% Micronized Talc FeaturesModified homopolymer and copolymer PP for injection moulding with the content of 40% micronized, chemically modified talc. Increased strength, rigidity and thermal application up to 130°C... |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 51 T 30 PP, 30% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 30% microground, floated, chemically modified talc. General application in all industry branches - packing material, garden.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PH 51 T 40 Polypropylene Homopolymer, 40% Micronized Talc FeaturesModified homopolymer PP for injection moulding with the content of 40% micronized, floated, chemically modified talc. General application in all industry branches - packing material, garden.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 61 B 70 PP, 70% mineral filling FeaturesModified PP for injection moulding with the content of 70% of barium sulphate. Increased density. Decreased shrinkage.Used for production of vertical blind weights. Delivered in natural mode.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PH 69 GF 30 Polypropylene Homopolymer, 30% Glass Fiber FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fiber, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 71 T 40 PP, 40% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc. General application in all industry branches - packing material, garden.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 76 FRD 3 PP, flame retardant FeaturesDetermined for environment, where contact with water is possible, because the electric properties do not change by conditioning. Application - terminals, coil forms, guides in washing machin.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PH 78 FRT 5 Polypropylene Homopolymer, Halogen Free and Phosphor Free Flame Retardant FeaturesModified homopolymer PP for injection moulding, contains the modifier of mechanical properties and non halogen and free phosphor flame retardant. Increased strength in comparison with unfil.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 78 T 40 PP, 40% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc. Stable towards detergents. General application in all industry branches.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 96 FRD 1 PP, flame retardant FeaturesDetermined for environment, where contact with water is possible, because the electric properties do not change by conditioning. Application - terminals, coil forms, guides in washing machin.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6 GF 20 LS PA6, 20% glass beads, light stability FeaturesStabilized against UV radiation. External use. PA 6 for injection moulding, reinforced with 20% glass beads offers high grade surface brightness, low rolling resistance force. Application: e.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature 23.0 °C |
0.476 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVASTYR® E BT N PET Basic type PET for injection molding, modified for general use, with excellent manufacturing properties. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fast.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVASTYR® E BT N PET Basic type PET for injection molding, modified for general use, with excellent manufacturing properties. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fast.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PH 49 GF 10 Polypropylene Homopolymer, 10% Glass Fiber FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 10% glass fiber, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 59 T 40 LW 031 PP, 40% mineral filling, laser label FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc.Contains modificator for laser labeling of finisched parts. /LASER NdIAG.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PH 91 T 20 Polypropylene Homopolymer, 20% Micronized Talc FeaturesModified homopolymer PP for injection moulding with the content of 20% micronized, floated, chemically modified talc. General application in all industry branches - packing material, garden.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 91 T 40 PP, 40% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc. General application in all industry branches - packing material, garden.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6 T 30 TS PA6, 30% mineral filling FeaturesDecreased shrinkage against the BT types, increased heat application. Increased modulus in tension - strength of the material. PA matrix reduction. PA for injection moulding with the content.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
|
LATI Latene® 22H2 MX/25 PP Homopolymer, Heat Stabilized Polypropylene homopolymer (PPh) based compound. Heat stabilized. Special mineral filler. Very good surface appearance.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
|
LATI Latigray 53/22-01 CX/25 PP Homopolymer, Impact Modified Radiopaque compound based on Polypropylene homopolymer (PPh), impact modified. Special mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformatio.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -30.0 °C |
0.476 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Noryl PKN4766 PPE+HIPS (Europe-Africa-Middle East) NORYL PKN4766 is a translucent PPO+PS extrusion grade for dilution with polystyrene resin. It is suitable for (microwavable) food packaging and is compliant with US and European food contact regulat.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature 23.0 °C |
0.476 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Borealis HK030U Polypropylene Compound HK030U is a special low viscosity polypropylene compound developed to fit the production of PP-GF composites in the direct LFT compression and injection molding process as well as in combination wit.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature 23.0 °C |
0.476 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Borealis HK060AE Polypropylene Homopolymer HK060AE is a special low viscosity polypropylene homopolymer compound developed to fit the production of glass matt reinforced thermoplastics. This material is also suitable as base resin for the pr.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature 23.0 °C |
0.476 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Unipetrol PE HD LITEN® BB 29 H HDPE Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature 23.0 °C |
0.476 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Unipetrol PE HD LITEN® VL 20 HDPE Extrusion and pipe applications.Information provided by Unipetrol RPA |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 72 T 20 PP, 20% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc conte nt. Decreased sh.. |