Plastics Group Polifil® 628-33GF Glass Fiber-Reinforced Nylon 6/6 (DAM)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer The Plastics Group of America
Trade Name Polifil®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastics Group Polifil® 628-33GF Glass Fiber-Reinforced Nylon 6/6 (DAM).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polifil® GFN/MRN 6/6 reinforced series of compounds offer superior strength, rigidity and creep resistance. Glass fibers provide excellent thermal and dimensional stability while maintaining good heat and chemical resistance.Applications: Bike componentsFuel capsAutomotive componentsStandard processing techniques are applicable.Information provided by The Plastics Group.
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
ASTM D792
Water Absorption 0.75 %
0.75 %
24 hours; ASTM D570
Linear Mold Shrinkage 0.0020 cm/cm

@Thickness 3.17 mm
0.0020 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength at Break 165 MPa
24000 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Elongation at Yield 3.0 %
3.0 %
ASTM D638
Flexural Strength 228 MPa
33000 psi
ASTM D790
Flexural Modulus 6.89 GPa
1000 ksi
Tangent; ASTM D790
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
At 73°F; ASTM D256
Thermal Properties Metric English Comments
Melting Point 254 °C
490 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 249 °C
480 °F
ASTM D648
Electrical Properties Metric English Comments
Dielectric Constant 3.7

@Frequency 1e+6 Hz
3.7

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 17.3 kV/mm
440 kV/in
ASTM D149
Users viewing this material also viewed the following: