Material Notes:
Property data is for samples at equilibrium moisture (2.0%)Information provided by PlastxWorld Inc.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Water Absorption 0.50 %
0.50 %
24 hr; ASTM D570
Moisture Absorption at Equilibrium 2.0 %
2.0 %
Mechanical Properties Metric English Comments
Tensile Strength at Break 32.4 MPa
4700 psi
ASTM D638
Flexural Yield Strength 44.8 MPa
6500 psi
ASTM D790
Flexural Modulus 1.50 GPa
218 ksi
ASTM D790
Izod Impact, Notched 3.20 J/cm
6.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 86.0 °C
187 °F
0.5 inch; ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in