Material Notes:
Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their performance under specific conditions. The manufacturing process for each grade is tightly controlled to produce materials that have a uniform microstructure and the right balance of strength, grain size and hardness to offer optimum performance for their intended applications.
Physical Properties Metric English Comments
Apparent Bulk Density 1.77 g/cc
0.0639 lb/in³
Particle Size 4.0 µm
4.0 µm
Mechanical Properties Metric English Comments
Hardness, Shore D 74
74
Tensile Strength, Yield 60.0 MPa
8700 psi
Estimated at 70% of flexural strength
Flexural Strength 85.0 MPa
12300 psi
Compressive Strength 140 MPa
20300 psi
Thermal Properties Metric English Comments
CTE, linear 8.10 µm/m-°C
4.50 µin/in-°F
Thermal Conductivity 95.0 W/m-K
659 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 0.00150 ohm-cm
0.00150 ohm-cm
Descriptive Properties Value Comments
Oxidation Threshold 440°C
Temperature that results in 1% weight loss in 24 hours. Oxidation threshold increases by approximately 100°C if graphite is purified.