Polymer Property : Apparent Bulk Density = 0.0639 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Apparent Bulk Density 1.77 g/cc
0.0639 lb/in³
Poco Graphite ACF-10Q Industrial Grade Graphite
POCO’s specialty graphite materials are used in a wide range of highly technical and industrial applications. Each grade has characteristics and properties that allow the user to match the ideal gr..
Apparent Bulk Density 1.77 g/cc
0.0639 lb/in³
Poco Graphite DFP Semiconductor Grade Graphite
Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their ..
Apparent Bulk Density 1.77 g/cc
0.0639 lb/in³
Poco Graphite Glassmate® LT Graphite
In very high wear situations, LT, with a hardness rating higher than GM material, will resist wear longer.
Apparent Bulk Density 1.77 g/cc
0.0639 lb/in³
Poco Graphite SCF Semiconductor Grade Graphite
Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their ..
Apparent Bulk Density 1.77 g/cc
0.0639 lb/in³
Poco Graphite SCF-2 Ion Implant Grade Graphite
An economic alternative to DFP-3-2, this 5-micron material is harder than DFP-3-2 and has high strengths without reduced porosity.
Apparent Bulk Density 1.77 g/cc
0.0639 lb/in³
Poco Graphite HPD Semiconductor Grade Graphite
Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their ..
Apparent Bulk Density 1.77 g/cc
0.0639 lb/in³
Poco Graphite ZEE-2 Ion Implant Grade Graphite
ZEE is a hard, wear-resistant material. This next generation ion implant material offers improved performance through the entire range of low to high-energy implants. POCO ZEE is high-purity, isotro..