Poco Graphite Glassmate® SR Graphite

Category Carbon , Graphite
Manufacturer Poco Graphite
Trade Name Glassmate®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Poco Graphite Glassmate® SR Graphite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
An economical material for short production runs. An ideal insert material for thick bead transfer applications.
Physical Properties Metric English Comments
Apparent Bulk Density 1.80 g/cc
0.0650 lb/in³
Particle Size 10 µm
10 µm
Mechanical Properties Metric English Comments
Hardness, Shore D 68
68
Flexural Strength 58.0 MPa
8410 psi
Compressive Strength 108 MPa
15700 psi
Thermal Properties Metric English Comments
CTE, linear 8.30 µm/m-°C
4.61 µin/in-°F
Thermal Conductivity 98.0 W/m-K
680 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 0.00146 ohm-cm
0.00146 ohm-cm
Descriptive Properties Value Comments
Oxidation Threshold 460°C