Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Strength = 108 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 108 MPa
15700 psi
20% pressing; EN ISO 604
Schwartz Technical Plastics LAMIGAMID® 320 Cast Polyamide 6, Conditioned
Application: heavy-duty wheelsInformation provided by Schwartz Technical Plastics GmbH
Compressive Strength 108 MPa
15700 psi
20% pressing; EN ISO 604
Schwartz Technical Plastics LAMIGAMID® 320 Cast Polyamide 6, Dry
Application: heavy-duty wheelsInformation provided by Schwartz Technical Plastics GmbH
Compressive Strength 108 MPa

@Time 36.0 sec
15700 psi

@Time 0.0100 hour
Wolf Kunststoff ZEDEX® ZX-410V7T A4T Polymer Alloy, Fiber Reinforced, Friction Modified
Main Characteristics: Fiber-reinforced; Friction-modified; Very high stiffness (higher than that of fiber-reinforced PEEK); Very low thermal expansion coefficient; Low friction; High wear resistance..
Compressive Strength 108 MPa

@Time 360000 sec
15700 psi

@Time 100 hour
Wolf Kunststoff ZEDEX® ZX-530CD3 031 Polymer Alloy, Fiber Reinforced and PTFE Modified
Main Characteristics: Dimensionally stable and rigid; Stress resistant; Extremely low wear to 100 ° CApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsIn..
Compressive Strength 108 MPa

@Time 36.0 sec
15700 psi

@Time 0.0100 hour
Wolf Kunststoff ZEDEX® ZX-750V5KF 055 Polymer Alloy. Fiber Reinforced
Main Characteristics: Stiff; High elongation and yield stress; Low thermal expansion; Impact resistantApplications: Textile Machinery; Compressors; Hinges; Handling; Machine Tools; Automitve Technol..
Compressive Strength 108 MPa
15600 psi
Cold Crushing Strength
Chosun Refractories BTB-18SC Casting Block
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 108 MPa
15600 psi
Cold Crushing Strength
Chosun Refractories SAL90N Special High Alumina brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 108 MPa
15600 psi
Cold Crushing Strength
Chosun Refractories SAL90Z Special High Alumina brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 108 MPa
15600 psi
10% deformation; ASTM D695
Beijing Ranger Chem BLUESTAR® BS450 Acetal Copolymer
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Compressive Strength 108 MPa
15700 psi
Abatron AboCast/AboCure 4-4/50-12 Casting Epoxy for Tooling
Standard casting compound for molds or patterns of any size, that can be machined with common metal working tools, engraving and reproduction molds.Main Advantages: FastBest rigid, chemical, and hea..
Compressive Strength 108 MPa
15600 psi
10% deformation; ASTM D695
Beijing Ranger Chem BLUESTAR® BS350 Acetal Copolymer
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Compressive Strength 108 MPa
15700 psi
Poco Graphite Glassmate® SR Graphite
An economical material for short production runs. An ideal insert material for thick bead transfer applications.
Copyright © lookpolymers.com All Rights Reserved