Polikim POLITAL® Polyoxymethylene (POM)

Category Polymer , Thermoplastic , Acetal (POM)
Manufacturer Polikim Polimer ve Kimya Sanay
Trade Name POLITAL®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polikim POLITAL® Polyoxymethylene (POM).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polital® is completely resistant to solvents, petroleum products, oil and grease. It is not resistant to strong acids, bases and oxidants. As it is affected by UV rays, its use in open air is not recommended. Applications: Gears, Guides, Cams, Electrical insulation, Conveyor components, Machine components, Bearings, Bolts, nuts, Hinges, junctures, Components subject to wear in humid environments or waterInformation provided by Polikim Polimer.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
ISO 1183
Water Absorption at Saturation 0.90 %
0.90 %
ISO 62
Mechanical Properties Metric English Comments
Hardness, Shore D 83
83
ISO 868
Tensile Strength, Ultimate 61.8 MPa
8960 psi
ISO 527
Elongation at Break 30 %
30 %
ISO 527
Tensile Modulus 2.80 GPa
406 ksi
ISO 527
Izod Impact, Notched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
ISO 180
Charpy Impact Unnotched NB
NB
ISO 179
Coefficient of Friction 0.30
0.30
Thermal Properties Metric English Comments
CTE, linear 100 µm/m-°C
55.6 µin/in-°F
ISO 11359
Thermal Conductivity 0.310 W/m-K
2.15 BTU-in/hr-ft²-°F
ISO 8301
Melting Point 168 °C
334 °F
Maximum Service Temperature, Air 90.0 °C
194 °F
continuous
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 55.0 kV/mm
1400 kV/in
ISO 60243