Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polikim ULPOLEN® 1000 UHMWPE, Oil

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), UHMW PE Ultra High Molecular Weight
Manufacturer Polikim Polimer ve Kimya Sanay
Trade Name ULPOLEN®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polikim ULPOLEN® 1000 UHMWPE, Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The solid lubricant additive reduces Ulpolen®'s coefficient of friction even further. As the additive is dry, it does not accumulate dust or dirt. In conveyor belts, it reduces squeakings at corners and turns. Especially in bottling, it helps reduce material waste and noise.Information provided by Polikim Polimer.
Physical Properties Metric English Comments
Density 0.955 g/cc
0.0345 lb/in³
ISO 1183
Molecular Weight 9.20e+6 g/mol
9.20e+6 g/mol
Mechanical Properties Metric English Comments
Hardness, Shore D 64
64
ISO 868
Tensile Strength, Ultimate 21.0 MPa
3040 psi
ISO 527-1
Elongation at Break >= 50 %
>= 50 %
ISO 527-1
Tensile Modulus 0.850 GPa
123 ksi
ISO 527-1
Coefficient of Friction 0.070
0.070
Sand Slurry 90
90
Thermal Properties Metric English Comments
CTE, linear 200 µm/m-°C

@Temperature 20.0 - 100 °C
111 µin/in-°F

@Temperature 68.0 - 212 °F
DIN 53752
Melting Point 133 - 138 °C
271 - 280 °F
Maximum Service Temperature, Air 80.0 °C
176 °F
continuous
130 °C
266 °F
short term
Minimum Service Temperature, Air -250 °C
-418 °F
-250 °C
-418 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
DIN VDE 0303
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
DIN VDE 0303
Arc Resistance 180 - 240 sec
180 - 240 sec
DIN VDE 0303
Users viewing this material also viewed the following: