Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.850 GPa | 123 ksi | |
Plastcom SLOVALEN EQ 18 N PP, basic type FeaturesModified PE with special heat and processional stabilization. Application in extrusion of profiles and pipes, blowing of bottles and jerrycans. Delivered in black colour.Packaging, transport.. |
|||
Tensile Modulus | 0.850 GPa @Thickness 2.00 mm |
123 ksi @Thickness 0.0787 in |
ISO 527-2 |
SABIC P5510 Black High Density Polyethylene for Pipes Product Description: P5510 is a black compound high density (class MRS 8 - PE 80) polyethylene with bimodal distribution of molecular mass. It is specifically designed for Pressure Pipe applicatio.. |
|||
Tensile Modulus | 0.850 GPa | 123 ksi | |
Radici Radilon® A USZ200 (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Tensile Modulus | 0.850 GPa | 123 ksi | ISO 527-1 |
Polikim ULPOLEN® 1000 UHMWPE, Oil The solid lubricant additive reduces Ulpolen®'s coefficient of friction even further. As the additive is dry, it does not accumulate dust or dirt. In conveyor belts, it reduces squeakings at corner.. |
|||
Tensile Modulus | 0.850 GPa | 123 ksi | |
LyondellBasell Lupolen® 4261 A HDPE, Blow Molding Grade Easy-to-process bow molding grade for technical containers such as fuel tanks, petrol filler inlets, expansion tanks, horticultural spray tanks, tanks for lawnmowers, disposable containers (up to 10.. |
|||
Tensile Modulus | 0.850 GPa | 123 ksi | 1 mm/min; ISO 527-1,-2 |
Inno-Comp INNOPOL® CS 2-8302 Elastomer Modified Polypropylene Block-Copolymer INNOPOL® CS 2-8302 is an elastomer modified compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-8302 is developed for extru.. |
|||
Tensile Modulus | 0.850 GPa | 123 ksi | ISO 527 |
Iran Petrochemical (PCC) EX 3 - 80 High Density Polyethylene EX3-80 is a high density polyethylene with 1-Butene as co monomer. It is natural, good ESCR, good impact strength, tough and rigid pipe resin. Applications: pipe extrusion PE 80 class, industrial a.. |
|||
Tensile Modulus | 0.850 GPa | 123 ksi | ISO 527 |
Iran Petrochemical (PCC) EX 3 – 100S HM CRP 100 N High Density Polyethylene EX3-100S is a high density polyethylene with 1-Butene as co monomer. It is natural, outstanding ESCR, high impact strength, outstanding hydrostatic strength for PE 100 class.Applications: pipe extr.. |
|||
Tensile Modulus | 0.850 GPa | 123 ksi | ISO 527-1 |
Iran Petrochemical (PCC) EX3 HM 5010 T2N High Density Polyethylene EX3 (HM 5010 T2N) is a natural colored high density polyethylene with Butene-1 as comonomer. The product is classified as PE 80 and good stress crack resistance properties combined with good impact .. |
|||
Tensile Modulus | >= 0.850 GPa | >= 123 ksi | 1 mm/min; ISO 527 |
MTM Plastics Purpolen® PE Polyethylene Regrind Purpolen® is a sorted regrind material suited to the production of demanding end user products. Extrusion and injection molding grades are available in many colors. The basis of our Purpolen® .. |
|||
Tensile Modulus | 0.850 GPa | 123 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics SABIC PPCOMPOUND 5521 PP SABIC® PPcompound 5521 is a mineral filled, impact modified polypropylene TPO. This material combines good flow with exterior automotive weathering stability. The general purpose black color prod.. |
|||
Tensile Modulus | 0.850 GPa | 123 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP TH0450A PUR LNP THERMOCOMP* TH0450A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Tensile Modulus | 0.850 GPa | 123 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP TH0450A PUR (Asia Pacific) LNP THERMOCOMP* TH0450A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Tensile Modulus | 0.850 GPa | 123 ksi | At 1 mm/min; ISO 527-2 |
Borealis Borstar® MB7541 High Density Polyethylene for Injection Molding Borstar MB7541 is a bimodal, natural, high density polyethylene produced by the Borstar PE technology. Borstar MB7541 combines excellent organoleptic properties, Environmental Stress Crack Resistan.. |
|||
Tensile Modulus | 0.850 GPa | 123 ksi | DIN EN ISO 527 |
Wolf Kunststoff ZEDEX® ZX-550PV A7A Polymer Alloy Main Characteristics: Modified friction wear; Tough; Soft; Reduced wear at temperatures at 100 ° CApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsInfor.. |
|||
Tensile Modulus | 0.850 GPa | 123 ksi | At 1 mm/min; ISO 527-2 |
Borealis Borstar® MB7542 High Density Polyethylene for Injection Molding Borstar MB7541 is a bimodal, natural, high density polyethylene produced by the Borstar PE technology. Borstar MB7541 combines excellent organoleptic properties, Environmental Stress Crack Resistan.. |
|||
Tensile Modulus | 0.850 GPa | 123 ksi | ISO 527 |
Borealis Daploy™ SF203HMS High Melt Strength Polypropylene for Extrusion Coating Daploy SF203HMS resin is a statistic-heterophasic-propylene-ethylene copolymer modified with a polypropylene based structurally isomeric polymer which combines a significantly increased melt strengt.. |
|||
Tensile Modulus | 0.850 GPa | 123 ksi | 1mm/min; ISO 527-2 |
Borealis RG435MO Polypropylene, Transparent Random Copolymer RG435MO is a specially modified highly-transparent polypropylene random copolymer with medium melt flow rate. Products molded from this grade exhibit excellent transparency, good gloss, high impact.. |
|||
Tensile Modulus | 0.850 GPa | 123 ksi | Film M.D.; ASTM D882 |
Eastman Embrace HY1000 Copolyester for Shrink Film Applications:Beverage packagingCosmetics/personal care packagingDairy packagingFood packagingJuice packagingPharmaceutical packagingKey Attributes:Eye catching 360° graphic capabilityNoise-free shr.. |
|||
Tensile Modulus | 0.850 GPa @Temperature 23.0 °C |
123 ksi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® ST811HS BK038 Nylon 6
(Unverified Data**) Zytel® ST811HS BK038 is a flexible, non-plasticized, black Super Tough nylon 6 resin developed for extrusion and injection molding applications such as cable and rope jacketing, hose inner cores an.. |
|||
Tensile Modulus | 0.850 GPa | 123 ksi | ASTM D638 |
Azdel SuperLite® SL551600-100 PP Resin Matrix / 55% Glass Fiber (9 mm Molded Thickness) AZDEL SuperLite® SL551600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Tensile Modulus | 0.850 GPa | 123 ksi | |
BASF Procom® X5S 770 Polypropylene Car bumpers and spoilers where good paintability is required.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 0.850 GPa | 123 ksi | At 1 mm/min; ISO 527-2 |
Borealis Bormed™ HE7541-PH HDPE for Healthcare Applications Bormed HE7541-PH is a bimodal, natural, high-density polyethylene produced by the Borstar PE technology. Bormed HE7541-PH combines low volatiles with high Environmental Stress Crack Resistance (ESC.. |
|||
Tensile Modulus | 0.850 GPa | 123 ksi | 1mm/min; ISO 527-2 |
Borealis Borpact™ SG930MO Polypropylene Copolymer Borpact™ SG930MO is a random heterophasic copolymer intended for injection molding. This grade yields high transparency and deep freeze impact resistance combined with excellent flow properties. an.. |