Polimeri Europa Riblene® MV 10 Low Density Polyethylene - Injection Molding

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer Polimeri Europa (Former EniChem)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Riblene® MV 10 Low Density Polyethylene - Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Riblene MV 10 is a low density polyethylene resin (LDPE) having an excellent fluidity.Parts made with Riblene MV 10 are highly flexible.Main Applications: Riblene MV 10 is ideal for injection molding applications. Riblene MV 10 is recommended for low thickness and very complex articles requiring a short production cycle and for masterbatches.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Specific Gravity 0.917 g/cc
0.917 g/cc
ISO 1183
Melt Flow 65 g/10 min

@Load 2.16 kg,
Temperature 190 °C
65 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 43
43
ISO 868/A
Tensile Strength, Yield 9.00 MPa
1310 psi
ISO 527
Flexural Modulus 0.110 GPa
16.0 ksi
ISO 178
Thermal Properties Metric English Comments
Melting Point 104 °C
219 °F
Internal method
Vicat Softening Point 80.0 °C

@Load 1.00 kg
176 °F

@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= 0.000 °C
<= 32.0 °F
ASTM D746