Polimeros Mexicanos Rotolene® Black Plus Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Polimeros Mexicanos
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeros Mexicanos Rotolene® Black Plus Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polyethylene compound specially formulated for rotational molding applications requiring good mechanical properties and good mold release properties. Rotational molded parts have smooth surface and texture finish when produced under optimal process conditions.Formulated for manufacturing water tanks (less than 1200 liters capacity)offering good mechanical properties and durability.Meets CONEG regulation for articles intended for direct food contact.Information provided by Polimeros Mexicanos
Physical Properties Metric English Comments
Bulk Density 0.330 - 0.390 g/cc
0.0119 - 0.0141 lb/in³
ASTM D1895
Density 0.937 g/cc
0.0339 lb/in³
ASTM D792
Particle Mesh Size 35 Mesh
35 Mesh
less than 2%; ASTM D1921
Melt Flow 4.0 - 5.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.0 - 5.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Impact Test 61.0 J

@Temperature -40.0 °C
45.0 ft-lb

@Temperature -40.0 °F
0.125 in.; ARM test
Descriptive Properties Value Comments
Pourability 2.5 - 4 gr/s
Process Rotational Molding