PolyMirae Moplen EP300L Injection Molding Grade Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer PolyMirae Company Ltd.
Trade Name Moplen
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyMirae Moplen EP300L Injection Molding Grade Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Moplen EP300L is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP300L is a block copolymer selected by customers for use in injection molding of toys, crates, battery case. Moplen EP300L resin meets the FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for food contact. Moplen EP300L has a flame rating of UL94HB.Features: Optimized balance of stiffness and toughness; High impact strength at low temperature; High stiffness; Low warpageApplications: Toy; Pail; Crate; HousewareInformation provided by PolyMirae Company Ltd.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ASTM D785
Tensile Strength, Yield 25.5 MPa
3700 psi
ASTM D638
Elongation at Yield 6.0 %
6.0 %
ASTM D638
Flexural Modulus 1.03 GPa
149 ksi
ASTM D790
Izod Impact, Notched 0.785 J/cm

@Temperature -20.0 °C
1.47 ft-lb/in

@Temperature -4.00 °F
ASTM D256
4.90 J/cm

@Temperature 23.0 °C
9.18 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
ASTM D648
Vicat Softening Point 150 °C
302 °F
ASTM D1525
Flammability, UL94 HB
HB