Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Edgetek® AT-10GB/000 Acetal-Copolymer, Glass Bead Filled  (discontinued **)

Category Polymer , Thermoplastic , Acetal (POM)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® AT-10GB/000 Acetal-Copolymer, Glass Bead Filled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description/Features:Glass Bead FilledPolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.47 g/cc
1.47 g/cc
ASTM D792
Water Absorption 0.20 %

@Thickness 3.17 mm
0.20 %

@Thickness 0.125 in
24 hr. Immersion; ASTM D570
Linear Mold Shrinkage 0.021 cm/cm
0.021 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 108
108
ASTM D785
Tensile Strength, Yield 48.3 MPa
7000 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Elongation at Yield 10 %
10 %
Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 3.10 GPa
450 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Izod Impact, Notched 0.534 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
1.00 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
230 °F
Unannealed, 0.125 in bars; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
ASTM D257
Processing Properties Metric English Comments
Melt Temperature 188 - 210 °C
370 - 410 °F
Molding
Mold Temperature 54.4 - 76.7 °C
130 - 170 °F
Drying Temperature 82.2 °C
180 °F
Dry Time 2 hour
2 hour
Descriptive Properties Value Comments
Product Form Pellets
Users viewing this material also viewed the following: