Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Edgetek® CY-1000 UV FR V0 Acrylonitrile Butadiene Styrene + PC (ABS+PC)

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate (PC)
Manufacturer PolyOne Corporation
Trade Name Edgetek®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® CY-1000 UV FR V0 Acrylonitrile Butadiene Styrene + PC (ABS+PC).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for elevated service temperature environments, high-modulus / structural materials for load-bearing and high-strength applications and flame-retardant products. These compounds are based on select engineering thermoplastic resins that are compounded with reinforcing additives such as carbon fiber, glass fiber and glass beads.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Water Absorption 0.10 %
0.10 %
@ 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 58.6 MPa
8500 psi
ASTM D638
Elongation at Break 10 %
10 %
Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 2.14 GPa
310 ksi
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 96.5 MPa
14000 psi
ASTM D790
Flexural Modulus 2.62 GPa
380 ksi
ASTM D790
Izod Impact, Notched 1.10 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
2.06 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 65.6 °C
150 °F
Unannealed; ASTM D648
Flammability, UL94 V-0

@Thickness 1.59 mm
V-0

@Thickness 0.0626 in
ALL; Internal Method
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+17 ohm-cm
1.00e+17 ohm-cm
ASTM D257
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
ASTM D257
Descriptive Properties Value Comments
Features Flame Retardant
Forms Pellets
Generic Material ABS+PC
Generic Name Acrylonitrile Butadiene Styrene + PC (ABS+PC)
Outdoor Suitability f2
UL 746C
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
RoHS Compliance RoHS Compliant
Users viewing this material also viewed the following: