Material Notes:
An excellent choice for low-voltage power-and-cable control cables, this RoHS compliant, flexible, black colored thermoplastic CPE jacketing compound offers wire and cable manufacturers the advantages of thermoplastic extrusion processing without the need to invest in continuous vulcanizing (CV) equipment. XCPE 32-33 RoHS Black is excellent for larger-diameter cables and co-extrusion strips for cable jacketing. Good heat/shock resistance, weatherability, moisture, oil and electrical properties as well as good processibility for high cable extrusion line speed.Note: Pre-drying is recommended for 4 hours at 175°-185°F. Note: Typical processing temperatures range between 320°-390°F depending upon screw design. Contact Technical Service for recommendation for specific equipment. NOTE: Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
ASTM D792
Melt Flow 15 g/10 min

@Load 21.6 kg,
Temperature 190 °C
15 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 39
39
Instant; ASTM D2240
Tensile Strength at Break 11.0 MPa
1600 psi
Type IV2 in/min; ASTM D638
Elongation at Break 450 %
450 %
Type IV, 51 mm/min; ASTM D638
Flexural Modulus 0.00641 GPa
0.930 ksi
13 mm/min; ASTM D790
Thermal Properties Metric English Comments
Brittleness Temperature -36.1 °C
-33.0 °F
ASTM D746
Oxygen Index 32 %

@Thickness 1.91 mm
32 %

@Thickness 0.0752 in
ASTM D2863
Descriptive Properties Value Comments
Appearance Pellets/Cubes
ASTM D2090
Forms Pellets
Generic Material CPE
Generic Name Polyethylene, Chlorinated (CPE)
Regional Availability Asia Pacific
North America
South America
RoHS Compliance RoHS Compliant
Uses Cable Jacketing