PolyOne Geon™ Vinyl Flexible B85UB Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Flexible B85UB Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 83
83
15 sec; ASTM D2240
90
90
ASTM D2240
Tensile Strength at Break 17.0 MPa
2470 psi
510 mm/min; ASTM D638
Tensile Strength 10.3 MPa

@Strain 100 %
1490 psi

@Strain 100 %
510 mm/min; ASTM D638
Elongation at Break 360 %
360 %
510 mm/min; ASTM D638
Tear Strength 79.7 kN/m
455 pli
Die C, 2 in/min; ASTM D1004
Compression Set 35 %

@Temperature 23.0 °C,
Time 79200 sec
35 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
Clash Berg Modulus 0.536 GPa
77.7 ksi
ASTM D1043
0.310 GPa

@Temperature -27.0 °C
45.0 ksi

@Temperature -16.6 °F
ASTM D1043
Thermal Properties Metric English Comments
Brittleness Temperature -29.0 °C
-20.2 °F
ASTM D746
Processing Properties Metric English Comments
Melt Temperature 171 - 177 °C
340 - 351 °F
193 - 199 °C
379 - 390 °F
Descriptive Properties Value Comments
Additive Biocide
UV Stabilizer
Features Medium Gloss
UV Absorbing
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Coextrusion
Extrusion
Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Liners