PolyOne Geon™ Vinyl Flexible R252AE Polyvinyl Chloride + NBR (PVC+NBR)

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Flexible R252AE Polyvinyl Chloride + NBR (PVC+NBR).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.29 g/cc
1.29 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 83
83
15 sec; ASTM D2240
Tensile Strength at Break 15.9 MPa
2310 psi
Type IV, 510 mm/min; ASTM D638
Elongation at Break 350 %
350 %
Type IV, 510 mm/min; ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature -32.2 °C
-26.0 °F
ASTM D746
Processing Properties Metric English Comments
Melt Temperature 177 - 182 °C
351 - 360 °F
193 - 204 °C
379 - 399 °F
Descriptive Properties Value Comments
Forms Pellets
Generic Material PVC+NBR
Generic Name Polyvinyl Chloride + NBR (PVC+NBR)
Processing Method Coextrusion
Extrusion
Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Construction Applications
Flooring
Outdoor Applications