PolyOne Geon™ Vinyl Wire & Cable JLC31A Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Wire & Cable JLC31A Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
15 sec; ASTM D2240
88
88
ASTM D2240
Tensile Strength at Break 15.2 MPa
2200 psi
Type IV, 510 mm/min; ASTM D638
Elongation at Break 300 %
300 %
Type IV, 510 mm/min; ASTM D638
Tensile Modulus 0.00758 GPa
1.10 ksi
Type IV, 510 mm/min; ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 90.0 °C
194 °F
UL Temperature Rating
Brittleness Temperature -40.0 °C
-40.0 °F
ASTM D746
Oxygen Index 25 %

@Thickness 1.91 mm
25 %

@Thickness 0.0752 in
ASTM D2863
Descriptive Properties Value Comments
Additive Lead Stabilizer
Features Flame Retardant
Fungus Resistant
Low Temperature Resistant
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Retention of Tensile Elongation 80%
121°C, 1.91 mm; 168 hr, UL Standard
Uses Communication Wire Jacketing
Wire & Cable Applications