PolyOne Maxxam™ XN-418.G001-1000 Polypropylene Copolymer (PP Copolymer)

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer PolyOne Corporation
Trade Name Maxxam™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Maxxam™ XN-418.G001-1000 Polypropylene Copolymer (PP Copolymer).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium carbonate, glass and talc to provide a desired balance of properties including stiffness, durability, impact resistance and heat resistance. Custom grades are available with features such as UV stabilizers, heat stabilizers, custom color, high impact, etc.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.23 g/cc
1.23 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0080 - 0.012 cm/cm
0.0080 - 0.012 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 75
75
ASTM D785
Tensile Strength, Yield 17.2 MPa
2490 psi
Type I, 51 mm/min; ASTM D638
Elongation at Break 470 %
470 %
Type I, 51 mm/min; ASTM D638
Flexural Strength 25.9 MPa
3760 psi
ASTM D790
Flexural Modulus 1.79 GPa
260 ksi
ASTM D790
Izod Impact, Notched 0.750 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
1.41 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Gardner Impact 17.6 J

@Thickness 3.18 mm,
Temperature 23.0 °C
13.0 ft-lb

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 96.1 °C

@Thickness 3.18 mm
205 °F

@Thickness 0.125 in
Annealed; ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
ALL; UL 94
Descriptive Properties Value Comments
Appearance Natural Color
Features Copolymer
Medium Flow
Medium Impact Resistance
Filler / Reinforcement Calcium Carbonate Filler
Unspecified FillerReinfor., 40% Filler by Weight
Forms Pellets
Generic Material PP Copolymer
Generic Name Polypropylene Copolymer (PP Copolymer)
Regional Availability Africa & Middle East
Asia Pacific
Europe
South America
Uses Construction Applications
Consumer Applications
General Purpose
Industrial Applications