Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polykemi AB POLYfill PPC 200 E20 Polypropylene Copolymer, Elastomer Modified

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Polykemi AB
Trade Name POLYfill
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polykemi AB POLYfill PPC 200 E20 Polypropylene Copolymer, Elastomer Modified.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Polykemi AB
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183
Melt Index of Compound 20 g/10 min

@Load 2.16 kg,
Temperature 230 °C
20 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break <= 32.0 MPa
<= 4640 psi
ISO/R527
Elongation at Yield 17 %
17 %
ISO/R527
Flexural Strength <= 28.0 MPa
<= 4060 psi
ISO 178
Flexural Modulus 1.20 GPa

@Temperature 23.0 °C
174 ksi

@Temperature 73.4 °F
ISO 178
Charpy Impact, Notched 0.450 J/cm²

@Temperature -20.0 °C
2.14 ft-lb/in²

@Temperature -4.00 °F
ISO 179
2.00 J/cm²

@Temperature 23.0 °C
9.52 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Processing Properties Metric English Comments
Melt Temperature 180 - 230 °C
356 - 446 °F
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
Dry Time 2 - 4 hour
2 - 4 hour
in circulation dryer
2 - 4 hour
2 - 4 hour
in desiccant air dryer
Injection Pressure 40.0 - 70.0 MPa
5800 - 10200 psi
Back Pressure 1.00 - 1.50 MPa
145 - 218 psi
Descriptive Properties Value Comments
Holding Pressure () > 40
% of injection pressure
Injection Speed () Highest possible