Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyplastic Armlen® PP-10IM-901 Polypropylene, Mineral Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Mineral Reinforced
Manufacturer Polyplastic Group
Trade Name Armlen®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyplastic Armlen® PP-10IM-901 Polypropylene, Mineral Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by PolyPlastic Group.
Physical Properties Metric English Comments
Density 0.990 g/cc
0.0358 lb/in³
ISO 1183
Melt Flow 22 g/10 min

@Load 2.16 kg,
Temperature 230 °C
22 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 19.0 MPa
2760 psi
ISO 527
Elongation at Break 200 %
200 %
ISO 527
Elongation at Yield 5.7 %
5.7 %
ISO 527
Flexural Modulus 1.55 GPa
225 ksi
ISO 178
Izod Impact, Notched (ISO) 6.70 kJ/m²

@Temperature -20.0 °C
3.19 ft-lb/in²

@Temperature -4.00 °F
ISO 180/1eA
40.0 kJ/m²

@Temperature 23.0 °C
19.0 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1eA
Processing Properties Metric English Comments
Melt Temperature 230 - 240 °C
446 - 464 °F
Mold Temperature 60.0 °C
140 °F
Drying Temperature 80.0 °C

@Time 7200 sec
176 °F

@Time 2.00 hour